Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 1.40 g/micron | 35.6 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips 4610 LDPE High Clarity, Bakery Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Clarity, Very High Gloss, Medium Slip, No Antiblock, Good Stability at High Drawdown Speeds, Good Printability, Good Heat Seal CharacteristicsApplic.. |
|||
Dart Drop | 1.40 g/micron | 35.6 g/mil | 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips HiD® 9662 HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Dart Drop | 1.40 g/micron | 35.6 g/mil | F<sub>50</sub>; ASTM D 1709 |
Total PPR 6573XHC Polypropylene, Random Copolymer Film Grade Random copolymer film gradeColor - Low catalyst residuals in FINA 6573XHC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 6573XHC improves its clarity and .. |
|||
Dart Drop | 1.40 g/micron | 35.6 g/mil | 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips MarFlex® 9659 HDPE Blown Film Resin Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Dart Drop | 1.40 g/micron | 35.6 g/mil | |
Dow LDPE 752A Low Density Polyethylene, Film Grade DOW LDPE 752A resin is a drawdown film resin for thin gauge applications such as garment films. It contains high levels of both slip and antiblock additives. This material complies with U.S.FDA regu.. |