Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 11.6 g/micron | 295 g/mil | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Dart Drop | 11.6 g/micron | 295 g/mil | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ H5604F High Density Polyethylene Film Key Characteristics:High tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierRecommended Applications: Films for shopping bag, T-shirt bag, garbage bag, liner bagInfor.. |