Polymer Property : Dart Drop = 295 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 11.6 g/micron
295 g/mil
F-50 at 26 in.; ASTM D1709
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Dart Drop 11.6 g/micron
295 g/mil
ASTM D1709
SCG Chemicals EL-Leneâ„¢ H5604F High Density Polyethylene Film
Key Characteristics:High tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierRecommended Applications: Films for shopping bag, T-shirt bag, garbage bag, liner bagInfor..