Mechanical Properties Metric English Comments
Dart Drop 4.55 g/micron
116 g/mil
ASTM D1709
Braskem LH 0820/30 AF LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Lamination; heavy duty bags; blends with LDPE and HDPE; valvulated heavy duty bags. Information provided by Braske..