Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 4.55 g/micron | 116 g/mil | ASTM D1709 |
Braskem LH 0820/30 AF LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Lamination; heavy duty bags; blends with LDPE and HDPE; valvulated heavy duty bags. Information provided by Braske.. |