Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 68.0 g/micron
1730 g/mil
ASTM D1709A
Westlake Mxsten CV CV77515-F Plastomer  (discontinued **)
Mxsten CV plastomer CV77515-X is a polyethylene plastomer designed for blown film extrusion that contains medium slip and no antiblock additives. Films produced with this resin exhibit a very low s..