Material Notes:
Mxsten CV plastomer CV77515-X is a polyethylene plastomer designed for blown film extrusion that contains medium slip and no antiblock additives. Films produced with this resin exhibit a very low seal initiation temperature with a broad hot tack window. Other features of this resin include a high melting point.List of Applications:Blown FilmFood packagingInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D4883
Thickness 25.0 microns
0.984 mil
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 8.00 MPa
1160 psi
ASTM D882
Film Elongation at Break, MD 750 %
750 %
ASTM D882
Film Elongation at Break, TD 1050 %
1050 %
ASTM D882
Secant Modulus, MD 0.152 GPa
22.0 ksi
1% Secant; ASTM D882
Secant Modulus, TD 0.172 GPa
24.9 ksi
1% Secant; ASTM D882
Elmendorf Tear Strength MD 400 g
400 g
Elmendorf Tear Strength TD 550 g
550 g
Elmendorf Tear Strength, MD 16.0 g/micron
406 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 22.0 g/micron
559 g/mil
ASTM D1922
Dart Drop 68.0 g/micron
1730 g/mil
ASTM D1709A
Film Tensile Strength at Break, MD 56.0 MPa
8120 psi
ASTM D882
Film Tensile Strength at Break, TD 44.0 MPa
6380 psi
ASTM D882
Heat Seal Strength Initiation Temperature 88.0 °C
190 °F
200 g/in seal strength is achieved
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 60 %
60 %
at 45°; ASTM D2457