Mechanical Properties Metric English Comments
Dart Drop <= 2.46 g/micron
<= 62.5 g/mil
ASTM D1709
ExxonMobil LL 3402.48 Cast Film Resin  (discontinued **)
LL 3402.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex..
Dart Drop <= 2.46 g/micron
<= 62.5 g/mil
ASTM D1709
ExxonMobil LL 1235x70 Cast Film Resin  (discontinued **)
LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical
Dart Drop <= 2.46 g/micron
<= 62.5 g/mil
ASTM D1709
ExxonMobil LL 1237x98 Cast Film Resin  (discontinued **)
LL 1237x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical
Dart Drop 2.46 g/micron
62.5 g/mil
26 in. dart; ASTM D-1709, A
Bapolene® 200F Polyethylene, Film Grade
Bapolene LD200F is a general purpose low density polyethylene for blown film extrusion applications. It contains medium levels of slip/antiblock additives. This product meets FDA standards for foo..
Dart Drop <= 2.46 g/micron
<= 62.5 g/mil
ASTM D1709
ExxonMobil LL 3404.48 Cast Film Resin  (discontinued **)
LL 3404.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex..