Polymer Property : Dart Drop = 239 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 9.40 g/micron
239 g/mil
F<sub>50</sub>; ASTM D 1709
Total PPH 3230 Polypropylene, Blow Molding Grade
Homopolymer blow molding gradeLubricated - Fina 3230 offers superior core rod release, eliminating the need for additional lubricant.High Purity - Fina 3230 features minimum taste and odor and optim..
Dart Drop 9.40 g/micron
239 g/mil
F<sub>50</sub>; ASTM D 1709
Total PPR 3230XZ Polypropylene, Blow Molding Grade
Homopolymer Blow Molding GradeLubricated – FINA 3230XZ offers superior core road release, eliminating the need for additional lubricant.Antistat – FINA 3230XZ contains antistat to minimize dust ac..
Dart Drop 9.40 g/micron
239 g/mil
F<sub>50</sub>; ASTM D 1709
Total PPR 8573 Polypropylene, Film Extrusion Grade
Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m..
Dart Drop 9.40 g/micron
239 g/mil
F<sub>50</sub>; ASTM D 1709
Total PPR 8473 Polypropylene, Film Extrusion Grade
Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8473 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The very ..
Dart Drop 9.40 g/micron
239 g/mil
ASTM D1709B
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati..