Material Notes:
Homopolymer blow molding gradeLubricated - Fina 3230 offers superior core rod release, eliminating the need for additional lubricant.High Purity - Fina 3230 features minimum taste and odor and optimum thermal stability for superior color and processability.FDA - Fina 3230 complies with all applicable FDA regulations and may be used under these provisions for food contact and packaging.Recommended Applications - Fina 3230 is ideal for food, cosmetic and pharmaceutical injection blow molded containers.Processing - Fina 3230 resin processes on conventional blow molding equipment with typical melt temperatures of 390-450°F (199-232°C)Data provided by the manufacturer, Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Water Vapor Permeability 7.10 g mil/ (m2 day)

@Temperature 37.8 °C
0.458 g mil/ (100 in2 day)

@Temperature 100 °F
90% RH; ASTM E96
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 1.6 g/10 min
1.6 g/10 min
ASTM D1238L
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256A
Dart Drop 9.40 g/micron
239 g/mil
F<sub>50</sub>; ASTM D 1709
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 199 - 232 °C
390 - 450 °F
blow molding