Mechanical Properties Metric English Comments
Dart Drop 3.12 g/micron
79.2 g/mil
1.5" Dart, 26" Drop Height; ASTM D1709
Chevron Phillips MarFlex® 5428 LDPE Cast Film Resin
Resin Type: HomopolymerCharacteristics: Excellent OpenabilitySuited for high speed convertingGood clarityLow COFApplications: Bakery FilmBreak BagsInformation provided by Chevron Phillips.