Polymer Property : Dart Drop = 48.3 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 1.90 g/micron
48.3 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene CopolymerCharacteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsApplications:Bakery Films, Coextr..
Dart Drop 1.90 g/micron
48.3 g/mil
Dow LDPE 586A Low Density Polyethylene, Packaging Grade
DOW LDPE 586A resin is used for general purpose packaging applications. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulatio..
Dart Drop 1.90 g/micron
48.3 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 6335B LLDPE Cast/Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene Copolymer, Medium Slip Version of 6335Characteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applications, Lo..