Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 5.12 g/micron | 130 g/mil | 26 in (66 cm); ASTM D1709 |
Chevron Phillips MarFlex® HHM TR-130 MDPE Film Resin Medium density resin provides overall balance of tensile, impact, and tear properties in film. It is suited for merchandise, produce, and trash bags. Processing performance is excellent on high st.. |
|||
Dart Drop | 5.12 g/micron | 130 g/mil | ASTM D1709 |
Huntsman PE 1253 EVA Film Extrusion
(discontinued **) 2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to.. |