Polymer Property : Dart Drop = 600 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 23.6 g/micron
600 g/mil
ASTM D1709A
ExxonMobil Exceed™ 1318CA Blown Film Resin  (discontinued **)
Exceed 1318CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1318CA resin have outstanding tensile, impact strength and puncture. These superi..
Dart Drop 23.6 g/micron
600 g/mil
ASTM D1709
Chevron Phillips MarFlex® D139DK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Dart Drop 23.6 g/micron
600 g/mil
ASTM D1709
Chevron Phillips MarFlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Dart Drop 23.6 g/micron
600 g/mil
ASTM D1709
Chevron Phillips MarFlex® D143FK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Dart Drop 23.6 g/micron
600 g/mil
ASTM D1709
ExxonMobil HD 7960.13 HMW Blown Film Resin
Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 ..