Mechanical Properties Metric English Comments
Dart Drop 2.20 - 3.30 g/micron
55.9 - 83.8 g/mil
Average value: 2.78 g/micron Grade Count:4
Overview of materials for Low Density Polyethylene (LDPE), Liner Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Liner Grade". Each property range of values reported is minimum and max..