Overview of materials for Low Density Polyethylene (LDPE), Liner Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Liner Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Low Density Polyethylene (LDPE), Liner Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Liner Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.920 - 0.927 g/cc
0.0332 - 0.0335 lb/in³
Average value: 0.924 g/cc Grade Count:4
Melt Flow 1.20 - 2.00 g/10 min
1.20 - 2.00 g/10 min
Average value: 1.80 g/10 min Grade Count:4
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.160 - 0.170 GPa
23.2 - 24.7 ksi
Average value: 0.162 GPa Grade Count:4
Secant Modulus, TD 0.180 - 0.200 GPa
26.1 - 29.0 ksi
Average value: 0.185 GPa Grade Count:4
Coefficient of Friction 0.100 - 1.00
0.100 - 1.00
Average value: 0.425 Grade Count:4
Dart Drop 2.20 - 3.30 g/micron
55.9 - 83.8 g/mil
Average value: 2.78 g/micron Grade Count:4
Optical Properties Metric English Comments
Haze 8.00 - 15.0 %
8.00 - 15.0 %
Average value: 11.0 % Grade Count:4
Gloss 39.0 - 80.0 %
39.0 - 80.0 %
Average value: 60.0 % Grade Count:4
Processing Properties Metric English Comments
Melt Temperature 193 - 204 °C
379 - 399 °F
Average value: 199 °C Grade Count:4