Mechanical Properties Metric English Comments
1% Secant Modulus 1250 MPa
181000 psi
Crosshead Speed 0.5 in/min; ASTM D790
LyondellBasell Alathon® M5363 High Density Polyethylene
ApplicationsALATHON L 4912 is a high molecular weight, high density copolymer with a broad molecular weight distribution. This resin provides excellent stiffness and a good balance of film properti..
1% Secant Modulus 1250 MPa
181000 psi
0.5"/min; ASTM D790
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade
ALATHON M5370PX is a copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processability. T..