Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.152 MPa | 22.0 psi | Overlap, Acrylic, 50% RH |
3M 4200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds to wood, gelcoat and fiberglass. It forms watertight, weather-resistant seals on joints an.. |