Mechanical Properties Metric English Comments
Shear Strength 0.152 MPa
22.0 psi
Overlap, Acrylic, 50% RH
3M 4200 Marine Adhesive/Sealant Fast Cure
A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds to wood, gelcoat and fiberglass. It forms watertight, weather-resistant seals on joints an..