Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.600 - 4.00 MPa | 87.0 - 580 psi | Average value: 1.81 MPa Grade Count:9 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Shear Strength | 0.600 MPa @Thickness 12800 mm, Time 335000 sec |
87.0 psi @Thickness 504 in, Time 93.0 hour |
Overlap, 1/8" Birch/Birch |
3M Fastbond™ 4213-NF Industrial Adhesive 3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when.. |