Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.552 - 0.689 MPa | 80.0 - 100 psi | Overlap, SBR/Steel |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 0.552 - 0.689 MPa | 80.0 - 100 psi | Overlap, SBR/Steel |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |