Polymer Property : Shear Strength = 1.13 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 1.13 MPa
164 psi
Overlap, Steel
3M Scotch-Seal™ 1252 Tamper Proof Sealant
3M™ Scotch-Seal™ Tamper Proof Sealant 1252 is a fast drying, anti-tamper sealer which is fire retardant.Features: Can be applied over adjustable or removable parts to indicuate changes in adjustme..