Polymer Property : Shear Strength = 1.55 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 1.55 MPa
225 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 3/16 - 6.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 1.55 MPa
>= 225 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRH-10 - 1/8- 4.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 1.55 MPa
225 psi
Dow Corning 3-0105 AUTOMOTIVE SEALANT
One-part RTV, alkoxy cure, designed for automotive powertrain sealing applicationsInformation provided by Dow Corning