Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.55 MPa | 225 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 3/16 - 6.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | >= 1.55 MPa | >= 225 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® HRH-10 - 1/8- 4.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 1.55 MPa | 225 psi | |
Dow Corning 3-0105 AUTOMOTIVE SEALANT One-part RTV, alkoxy cure, designed for automotive powertrain sealing applicationsInformation provided by Dow Corning |