Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 73.8 - 91.7 MPa | 10700 - 13300 psi | Average value: 83.1 MPa Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |