Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.38 - 1.81 g/cc
0.0499 - 0.0654 lb/in³
Average value: 1.50 g/cc Grade Count:53
1.10 - 1.10 g/cc

@Temperature 325 - 325 °C
0.0397 - 0.0397 lb/in³

@Temperature 617 - 617 °F
Average value: 1.10 g/cc Grade Count:1
Filler Content 35.0 - 40.0 %
35.0 - 40.0 %
Average value: 38.9 % Grade Count:28
Water Absorption 0.0200 - 5.00 %
0.0200 - 5.00 %
Average value: 0.826 % Grade Count:14
1.10 - 1.15 %

@Temperature 70.0 - 70.0 °C
1.10 - 1.15 %

@Temperature 158 - 158 °F
Average value: 1.12 % Grade Count:6
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00374 cm/cm Grade Count:45
Linear Mold Shrinkage, Transverse 0.00450 - 0.105 cm/cm
0.00450 - 0.105 in/in
Average value: 0.00982 cm/cm Grade Count:19
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124 - 125
124 - 125
Average value: 125 Grade Count:8
Ball Indentation Hardness 310 - 330 MPa
45000 - 47900 psi
Average value: 322 MPa Grade Count:5
Tensile Strength, Ultimate 6.13 - 260 MPa
889 - 37700 psi
Average value: 180 MPa Grade Count:54
65.0 - 230 MPa

@Temperature -40.0 - 200 °C
9430 - 33400 psi

@Temperature -40.0 - 392 °F
Average value: 98.0 MPa Grade Count:4
120 - 130 MPa

@Temperature 130 - 180 °C
17400 - 18900 psi

@Temperature 266 - 356 °F
Average value: 98.0 MPa Grade Count:5
120 - 130 MPa

@Time 1.80e+7 - 7.20e+7 sec
17400 - 18900 psi

@Time 5000 - 20000 hour
Average value: 98.0 MPa Grade Count:5
3.94 - 237.87 MPa

@Strain 0.0400 - 5.10 %
571 - 34500 psi

@Strain 0.0400 - 5.10 %
Average value: 98.0 MPa Grade Count:2
3.94 - 237.87 MPa

@Temperature -20.0 - 180 °C
571 - 34500 psi

@Temperature -4.00 - 356 °F
Average value: 98.0 MPa Grade Count:2
Elongation at Break 1.00 - 4.50 %
1.00 - 4.50 %
Average value: 2.34 % Grade Count:55
2.10 - 8.60 %

@Temperature -40.0 - 200 °C
2.10 - 8.60 %

@Temperature -40.0 - 392 °F
Average value: 4.42 % Grade Count:4
Modulus of Elasticity 10.0 - 17.2 GPa
1450 - 2500 ksi
Average value: 12.8 GPa Grade Count:52
2.333 - 13.0 GPa

@Temperature -40.0 - 230 °C
338.4 - 1890 ksi

@Temperature -40.0 - 446 °F
Average value: 7.20 GPa Grade Count:8
Flexural Yield Strength 231 - 360 MPa
33500 - 52200 psi
Average value: 299 MPa Grade Count:33
261 - 352 MPa

@Temperature -40.0 - 60.0 °C
37900 - 51100 psi

@Temperature -40.0 - 140 °F
Average value: 154 MPa Grade Count:1
96.0 - 181 MPa

@Temperature 100 - 200 °C
13900 - 26300 psi

@Temperature 212 - 392 °F
Average value: 154 MPa Grade Count:2
96.0 - 181 MPa

@Strain 3.50 - 5.00 %
13900 - 26300 psi

@Strain 3.50 - 5.00 %
Average value: 154 MPa Grade Count:2
Flexural Modulus 8.30 - 15.9 GPa
1200 - 2300 ksi
Average value: 12.2 GPa Grade Count:38
3.46 - 10.62 GPa

@Temperature -40.0 - 200 °C
502 - 1540 ksi

@Temperature -40.0 - 392 °F
Average value: 5.77 GPa Grade Count:2
Compressive Yield Strength 71.0 - 355 MPa

@Temperature -40.0 - 200 °C
10300 - 51500 psi

@Temperature -40.0 - 392 °F
Average value: 171 MPa Grade Count:1
Poissons Ratio 0.380 - 0.390
0.380 - 0.390
Average value: 0.387 Grade Count:4
Shear Modulus >= 0.0768 GPa

@Temperature -50.0 - 290 °C
>= 11.1 ksi

@Temperature -58.0 - 554 °F
Average value: 1.60 GPa Grade Count:1
Shear Strength 73.8 - 91.7 MPa
10700 - 13300 psi
Average value: 83.1 MPa Grade Count:3
Secant Modulus 1.70799 - 14.8867 GPa

@Temperature 0.000 - 200 °C
247.727 - 2159.17 ksi

@Temperature 32.0 - 392 °F
Average value: 10.1 GPa Grade Count:1
1.70799 - 14.8867 GPa

@Strain 0.0500 - 4.13 %
247.727 - 2159.17 ksi

@Strain 0.0500 - 4.13 %
Average value: 10.1 GPa Grade Count:1
Izod Impact, Notched 0.650 - 2.94 J/cm
1.22 - 5.50 ft-lb/in
Average value: 1.21 J/cm Grade Count:19
0.910 - 0.910 J/cm

@Temperature -40.0 - -40.0 °C
1.70 - 1.70 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.910 J/cm Grade Count:1
Izod Impact, Unnotched 5.87 - 11.2 J/cm
11.0 - 21.0 ft-lb/in
Average value: 7.62 J/cm Grade Count:14
Izod Impact, Notched (ISO) 8.50 - 12.0 kJ/m²
4.04 - 5.71 ft-lb/in²
Average value: 10.2 kJ/m² Grade Count:8
8.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.33 kJ/m² Grade Count:2
Izod Impact, Unnotched (ISO) 40.0 - 65.0 kJ/m²
19.0 - 30.9 ft-lb/in²
Average value: 56.0 kJ/m² Grade Count:5
55.0 - 67.0 kJ/m²

@Temperature -30.0 - -30.0 °C
26.2 - 31.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 61.0 kJ/m² Grade Count:2
Charpy Impact Unnotched 3.80 - 9.00 J/cm²
18.1 - 42.8 ft-lb/in²
Average value: 6.26 J/cm² Grade Count:30
3.50 - 7.50 J/cm²

@Temperature -40.0 - -30.0 °C
16.7 - 35.7 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 5.25 J/cm² Grade Count:10
Charpy Impact, Notched 0.800 - 1.40 J/cm²
3.81 - 6.66 ft-lb/in²
Average value: 1.01 J/cm² Grade Count:30
0.600 - 1.10 J/cm²

@Temperature -40.0 - -30.0 °C
2.86 - 5.24 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.921 J/cm² Grade Count:11
Tensile Creep Modulus, 1 hour 10000 - 11000 MPa
1.45e+6 - 1.60e+6 psi
Average value: 10500 MPa Grade Count:4
Tensile Creep Modulus, 1000 hours 8500 - 10000 MPa
1.23e+6 - 1.45e+6 psi
Average value: 9130 MPa Grade Count:4
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Average value: 1.00e+15 ohm-cm Grade Count:18
Surface Resistance 1.00e+13 - 1.00e+15 ohm
1.00e+13 - 1.00e+15 ohm
Average value: 3.85e+14 ohm Grade Count:5
Dielectric Constant 3.80 - 5.80
3.80 - 5.80
Average value: 4.30 Grade Count:8
4.20 - 136

@Temperature 60.0 - 200 °C
4.20 - 136

@Temperature 140 - 392 °F
Average value: 30.5 Grade Count:1
4.20 - 136

@Frequency 1000 - 1.00e+6 Hz
4.20 - 136

@Frequency 1000 - 1.00e+6 Hz
Average value: 30.5 Grade Count:1
Dielectric Strength 19.7 - 43.0 kV/mm
500 - 1090 kV/in
Average value: 33.0 kV/mm Grade Count:13
Users viewing this material also viewed the following: