Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 148 MPa @Thickness 15.7 mm |
21500 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP510A Glass Fabric Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-.. |
|||
Shear Strength | 148 MPa | 21500 psi | Punch test on film, unusually high for a polymer; ASTM D732 |
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |