Shear Strength 148 MPa

@Thickness 15.7 mm
21500 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP510A Glass Fabric
Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-..
Shear Strength 148 MPa
21500 psi
Punch test on film, unusually high for a polymer; ASTM D732
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..