Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 44.1 - 108 MPa | 6400 - 15700 psi | Average value: 79.2 MPa Grade Count:53 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Shear Strength | 75.8 - 108 MPa | 11000 - 15700 psi | Average value: 91.3 MPa Grade Count:8 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |