Polymer Property : Shear Strength = 16.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 1.38 - 16.5 MPa
200 - 2400 psi
ITW Plexus Plexusâ„¢ MA820 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent for structural bonding of surface metals with no surface preparation.Information provide..