Mechanical Properties Metric English Comments
Shear Strength 16.8 MPa
2440 psi
Overlap, Steel to Steel
3M Scotch-Weld™ 1751 B/A Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1751 B/A is a gray, aluminum filled, two-part, room temperature curing structural adhesive.Information provided by 3M
Shear Strength 16.8 MPa

@Temperature 81.0 - 83.0 °C
2440 psi

@Temperature 178 - 181 °F
Etched Aluminum Overlap, 26% Methyl Alcohol/74% Tap Water Immersion for 30 days
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M
Shear Strength 16.8 MPa

@Temperature -253 °C
2440 psi

@Temperature -423 °F
Overlap, Etched Aluminum; ASTM D1002
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..