Polymer Property : Shear Strength = 164.095 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 11.0 - 164.095 MPa

@Temperature -55.0 - 177 °C
1600 - 23800.0 psi

@Temperature -67.0 - 351 °F
Average value: 58.8 MPa Grade Count:26
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..