Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 179 MPa @Thickness 1.57 mm |
26000 psi @Thickness 0.0620 in |
Perpendicular |
Industrial Laminates/Norplex NP190 Synthetic Fabric
(discontinued **) Description: Aramid fabric material with a high performance phenolic resin matrix. Excellent electrical and mechanical properties at elevated temperatures, and in adverse environments. Applications .. |
|||
Shear Strength | 179 MPa @Thickness 15.7 mm |
26000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP511ES Glass Epoxy Laminate Description: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a con.. |