Material Notes:
Description: Aramid fabric material with a high performance phenolic resin matrix. Excellent electrical and mechanical properties at elevated temperatures, and in adverse environments. Applications include wear plates for conveyor systems, and compressor and pump vanes.Thickness Tested: 0.125", 0.250" & 0.500"
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93 - 113

@Thickness 1.57 mm
93 - 113

@Thickness 0.0620 in
Flexural Strength 341 MPa

@Thickness 1.57 mm
49500 psi

@Thickness 0.0620 in
CW
461 MPa

@Thickness 1.57 mm
66800 psi

@Thickness 0.0620 in
LW
Compressive Strength 517 MPa

@Thickness 12.7 mm
75000 psi

@Thickness 0.500 in
Flatwise
Shear Strength 179 MPa

@Thickness 1.57 mm
26000 psi

@Thickness 0.0620 in
Perpendicular
Izod Impact, Unnotched 9.88 J/cm

@Thickness 12.7 mm
18.5 ft-lb/in

@Thickness 0.500 in
CW, E-48/50
10.7 J/cm

@Thickness 12.7 mm
20.0 ft-lb/in

@Thickness 0.500 in
LW, E-48/50
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Maximum Operating Temperature
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 5.19

@Thickness 1.57 mm
5.19

@Thickness 0.0620 in
Permittivity, Cond D-24/23
Dielectric Strength 9.53 kV/mm

@Thickness 1.57 mm
242 kV/in

@Thickness 0.0620 in
D-48/50
21.3 kV/mm

@Thickness 1.57 mm
540 kV/in

@Thickness 0.0620 in
Condition - A
Dielectric Breakdown 9000 V

@Thickness 1.57 mm
9000 V

@Thickness 0.0620 in
D-48/50
75000 V

@Thickness 1.57 mm
75000 V

@Thickness 0.0620 in
Condition A
Dissipation Factor 0.0461

@Thickness 1.57 mm
0.0461

@Thickness 0.0620 in
Cond D-24/23
Arc Resistance 182 sec

@Thickness 3.17 mm
182 sec

@Thickness 0.125 in
ASTM D495
Descriptive Properties Value Comments
Bond Strength 1,800 lb
0.5"