Polymer Property : Shear Strength = 17900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 123 MPa
17900 psi
ASTM D732
Haysite EMD Polyester, Glass Reinforced
EMD is a glass mat reinforced polyester sheet designed primarily as a "slot wedge" material in large motors and generators. EMD has low weight loss at elevated temperatures and high flexural and sh..