Material Notes:
EMD is a glass mat reinforced polyester sheet designed primarily as a "slot wedge" material in large motors and generators. EMD has low weight loss at elevated temperatures and high flexural and shear strength; properties required in demanding "slot wedge" applications. Available thicknesses - .062" - 1.00". Standard color - Black.Information provided by Haysite
Physical Properties Metric English Comments
Specific Gravity 1.94 g/cc
1.94 g/cc
ASTM D792
Water Absorption 0.19 %
0.19 %
ASTM D229
Mechanical Properties Metric English Comments
Hardness, Barcol 67
67
Tensile Strength 114 MPa
16500 psi
ASTM D638
Flexural Strength 228 MPa
33000 psi
ASTM D790
Flexural Modulus 12.4 GPa
1800 ksi
ASTM D790
Compressive Strength 359 MPa
52000 psi
ASTM D695
Shear Strength 123 MPa
17900 psi
ASTM D732
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
Edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 180 °C
356 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 4.8

@Frequency 60.0 Hz
4.8

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 16.7 kV/mm

@Thickness 1.59 mm
425 kV/in

@Thickness 0.0625 in
Perpendicular, Short Time in Oil; ASTM D149
Dielectric Breakdown 60000 V
60000 V
Parallel, Step-By-Step in Oil; ASTM D149
Dissipation Factor 0.020

@Frequency 60.0 Hz
0.020

@Frequency 60.0 Hz
ASTM D150
Arc Resistance 150 sec
150 sec
ASTM D495
Descriptive Properties Value Comments
Flame Resistance 287 seconds
Burning Time, ASTM D229
75 seconds
Ignition Time, ASTM D229
Users viewing this material also viewed the following: