Mechanical Properties Metric English Comments
Shear Strength 15.2 - 18.6 MPa
2200 - 2700 psi
ITW Plexus Plexusâ„¢ MA822 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Wo..