Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 19.0 MPa | 2750 psi | CRS Overlap, Tap Water at RT |
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Shear Strength | 19.0 MPa | 2750 psi | Overlap, CRS/CRS after 7 days of Immersion in Gasoline |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 19.0 MPa | 2750 psi | Overlap, Green Fiberglass Reinforced Plastic, Adhesive Failure |
3M Scotch-Weld™ DP812 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Shear Strength | 19.0 MPa | 2750 psi | Overlap at 2 hrs after bonding |
3M Scotch-Weld™ DP810 Tan Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 19.0 MPa @Temperature 81.0 - 83.0 °C |
2760 psi @Temperature 178 - 181 °F |
Etched Aluminum Overlap, Tap Water Immersion for 30 days |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Shear Strength | 19.0 MPa | 2750 psi | Overlap, Etched Al, JP-4 for 30 days |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |