Mechanical Properties Metric English Comments
Shear Strength >= 2.21 MPa
>= 320 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..
Shear Strength 2.21 MPa
320 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 1/4-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 2.21 MPa
>= 320 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRH-10/F50 - 5.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglass cloth reinforc..
Shear Strength 2.21 MPa
320 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRH-327 - 3/16 - 4.5 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Shear Strength 2.21 MPa
320 psi
Bond, Al to Al
Master Bond EP30ND Non-Drip, Dimensionally Stable Epoxy Adhesive
Description: Master Bond Polymer System EP30ND is a high viscosity, two component epoxy adhesive/sealant with a paste consistency. It will cure at room temperature or more rapidly at elevated temper..
Shear Strength 2.21 MPa
320 psi
Lap Shear Strength; ASTM D1002
Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Shear Strength 2.21 MPa
320 psi
Overlap, Isopropyl Alcohol Wipe surface prep, ABS PVC
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 2.21 MPa
320 psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polystyrene
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 2.21 MPa
320 psi
Overlap, Aluminum -120 frit sandpaper
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Shear Strength 2.21 MPa
320 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..