Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassProduct Use: Thermally conductive adhesiveAppearance: Gray gum on brown and clear linersThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 2.60 g/cc
0.0939 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Liner
76.2 microns
3.00 mil
Carrier
203 microns
8.00 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
Silicone Property; ASTM D2240
Tensile Strength 2.28 MPa
330 psi
Silicone Property; ASTM D412
Elongation at Break 170 %
170 %
Silicone Property; ASTM D412
Modulus of Elasticity 0.00159 GPa
0.230 ksi
Silicone Property; Arlon SQA-TMS-008
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Shear Modulus 0.345 GPa

@Strain <=100 %
50.0 ksi

@Strain <=100 %
ASTM D1002
Shear Strength 2.21 MPa
320 psi
Lap Shear Strength; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 128 µm/m-°C
71.1 µin/in-°F
Silicone Property; ASTM E 831
Specific Heat Capacity 0.900 J/g-°C

@Temperature 100 °C
0.215 BTU/lb-°F

@Temperature 212 °F
Silicone Property; ASTM E 1952
Thermal Conductivity 2.30 W/m-K
16.0 BTU-in/hr-ft²-°F
Product Property; ASTM E 1530
1.40 W/m-K

@Temperature 100 °C
9.72 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E 1530
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Glass Transition Temp, Tg -120 °C
-184 °F
Silicone Property; ASTM D3418
Electrical Properties Metric English Comments
Dielectric Constant 5.9

@Frequency 1.00e+6 Hz
5.9

@Frequency 1.00e+6 Hz
D<sub>k</sub>, Silicone Property; IPC TM 650-2.5.5.3
Dielectric Strength 33.5 kV/mm
850 kV/in
ASTM D149
Dissipation Factor 0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
D<sub>f</sub>, Silicone Property; IPC TM 650-2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min
0.250 hour
After Thermabond® temperature reaches 100°C, Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 4.44 - 10.0 °C
6.00 Month

@Temperature 40.0 - 50.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Gray
Plasticity 2.2 mm
Arlon SQA-TMS-005
Total Product Weight (g/m2) 528
Arlon SQA-TMS-025