Mechanical Properties Metric English Comments
Shear Strength 2.65 MPa
385 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRH-10 - 1/8- 6.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..