Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.65 MPa | 385 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/8- 6.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |