Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 15.5 MPa | 2250 psi | CRS Overlap, Hydraulic Oil at RT |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Shear Strength | 15.5 MPa | 2250 psi | CRS Overlap, Tap Water at RT |
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e.. |
|||
Shear Strength | 15.5 MPa | 2250 psi | Overlap, Etched Aluminum tested after 1 week of Immersion in 66°C tap water |
3M Scotch-Weld™ DP807 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Shear Strength | 15.5 MPa | 2250 psi | Overlap at 1 hr after bonding |
3M Scotch-Weld™ DP810 Tan Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 15.5 MPa @Time 1800 sec |
2250 psi @Time 0.500 hour |
Aluminum Overlap |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |