Material Notes:
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent environmental resistance. Excellent for bonding many metals, woods, rubbers and some plastics.Information provided by 3M
Physical Properties Metric English Comments
Viscosity 300000 - 1.00e+6 cP
300000 - 1.00e+6 cP
70000 - 6.00e+6 cP
70000 - 6.00e+6 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 85
80 - 85
Tensile Strength, Ultimate 29.6 MPa
4290 psi
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
Modulus of Elasticity 2.37 GPa
344 ksi
Shear Strength 7.58 MPa
1100 psi
CRS Overlap, White Gas @ RT
13.4 MPa
1950 psi
CRS Overlap, Tap Water at RT
13.8 - 15.2 MPa
2000 - 2200 psi
CRS Overlap
15.2 MPa
2200 psi
CRS Overlap, 100% RH at 49°C
15.5 MPa
2250 psi
CRS Overlap, Hydraulic Oil at RT
3.45 MPa

@Temperature 82.0 °C
500 psi

@Temperature 180 °F
Aluminum Overlap; ASTM D1002
10.3 MPa

@Temperature -55.0 °C
1500 psi

@Temperature -67.0 °F
Aluminum Overlap; ASTM D1002
20.7 MPa

@Temperature 24.0 °C
3000 psi

@Temperature 75.2 °F
Aluminum Overlap; ASTM D1002
Peel Strength 0.351 kN/m

@Temperature -55.0 °C
2.00 pli

@Temperature -67.0 °F
Aluminum T-Peel; ASTM D1876
0.701 kN/m

@Temperature 24.0 °C
4.00 pli

@Temperature 75.2 °F
Aluminum T-Peel; ASTM D1876
0.701 kN/m

@Temperature 82.0 °C
4.00 pli

@Temperature 180 °F
Aluminum T-Peel; ASTM D1876
Thermal Properties Metric English Comments
CTE, linear 79.0 µm/m-°C

@Temperature 0.000 - 40.0 °C
43.9 µin/in-°F

@Temperature 32.0 - 104 °F
Thermal Conductivity 0.293 W/m-K
2.03 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 55.0 °C
131 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+15 ohm-cm
1.50e+15 ohm-cm
Dielectric Constant 6.06

@Frequency 1000 Hz
6.06

@Frequency 1000 Hz
Dielectric Strength 23.0 kV/mm
585 kV/in
Dissipation Factor 0.012

@Frequency 1000 Hz
0.012

@Frequency 1000 Hz
Descriptive Properties Value Comments
Appearance Green
Accelerator
Green
White
Base