Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 16.3 MPa @Temperature 82.0 °C |
2360 psi @Temperature 180 °F |
Solvent Wiped Cold Rolled Steel Overlap |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |