Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 0.172 MPa | >= 24.9 psi | Cured; ASTM D1002 |
Parker Chomerics Tecknit® 72-00014 Silver-Filled Flexible Resin Caulking System Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide .. |