Parker Chomerics Tecknit® 72-00014 Silver-Filled Flexible Resin Caulking System

Category Polymer
Manufacturer Parker Chomerics
Trade Name Tecknit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit® 72-00014 Silver-Filled Flexible Resin Caulking System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide over 100 dB total shielding effectiveness across the RF spectrum. They may be used to improve joint or seam integrity for all types of electronic enclosures. An outstanding feature of these one-component systems is the ease with which they may be applied with conventional caulking guns and dispensing equipment, such as small bead orifice syringes. Hand application with spatula or putty knife is also simple. High yield per pound is another advantage offered in these conductive caulks. Proprietary formulation techniques result in lower density than most current state-of-the-art caulking compounds. The systems are safe to handle, very easily applied and free of any corrosive binders. They contain silver plated glass or copper particles for electrical conductivity, assuring stable operation over wide temperature ranges not generally possible with carbon- black filled systems.Application Information: This system is a conductive, fast room temperature curing silicone-silver caulking compound. Ease of application and high electrical conductivity are outstanding features of this flexible system. It is used to fill gaps in shielded room joints, repair damaged conductive gaskets and shield/seal permanently mounted panels, components and hardware. This system will withstand shock vibration, seam warpingInformation provided by Chomerics
Mechanical Properties Metric English Comments
Shear Strength >= 0.172 MPa
>= 24.9 psi
Cured; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Cured
Minimum Service Temperature, Air -63.0 °C
-81.4 °F
Cured
Shrinkage <= 26 %
<= 26 %
Cured
Electrical Properties Metric English Comments
Volume Resistivity <= 0.010 ohm-cm
<= 0.010 ohm-cm
Cured; QAP-1017
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Recommended Cure
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Full Cure
Shelf Life 9.00 Month
9.00 Month
Unopened Container
Descriptive Properties Value Comments
Color Tan
Consistency Self-Leveling
Filler Ag/Glass
Final Condition Flexible
Number of Components One
Resin Silicone
Volume 13.8 in3
Weight 16 oz