Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 25.3 MPa | 3670 psi | Etched Aluminum Overlap, 100% RH @ 49°C for 90 days |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |