Mechanical Properties Metric English Comments
Shear Strength 25.5 MPa
3700 psi
Interlaminar S23; ASTM D2344
Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..
Shear Strength 25.5 MPa
3700 psi
Tensile
Resin Technology Group Fusion 1 General Purpose Fusion Cyanoacrylate
Information provided by Resin Technology Group.
Shear Strength 25.5 MPa
3700 psi
ASTM D732
Spartech Polycast Poly 2000 (Mil-P-25690;Class 1) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Shear Strength 25.5 MPa
3700 psi
ASTM D732
Spartech Polycast Poly 2000 (Mil-P-25690;Class 2) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Shear Strength 25.5 MPa
3700 psi
Overlap at 2 hrs after bonding
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 25.5 MPa
3700 psi
Overlap, Aluminum, Cohesive Failure
3M Scotch-Weld™ DP8810NS Low Odor Acrylic Adhesives
3M™ Scotch-Weld™ Low Odor Acrylic Adhesives are high performance, two-part acrylic adhesives with lower odor than most acrylic adhesives. These toughened products offer excellent shear, peel, and ..
Shear Strength 25.5 MPa
3700 psi
Overlap, Etched Aluminum, 65°C/80% RH for 30 days, Cohesive Failure
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 25.5 MPa

@Temperature -55.0 °C
3700 psi

@Temperature -67.0 °F
Aluminum, Overlap; ASTM D1002
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..
Shear Strength 25.5 MPa
3700 psi
Overlap, Stainless Steel-MEK/Abrade/MEK, Cohesive/Adhesive Failure
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..