Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 29.6 MPa | 4300 psi | |
Indium Corp. Indalloy 5 Indium-Lead-Tin Solder Alloy Very good resistance to alkaline corrosionInformation Provided by Indium Corporation |
|||
Shear Strength | 29.6 MPa @Temperature 21.0 °C |
4300 psi @Temperature 69.8 °F |
Overlap |
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b.. |
|||
Shear Strength | 29.6 MPa @Temperature 218 °C |
4300 psi @Temperature 424 °F |
Bond Line |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |